SL-D001 Pattern Wax is a non-filled pattern wax for art casting. This wax is produced with high production technology. The patterns can be accurately and consistently produced to tight tolerances.
Features
EXCELLENT DIMENSIONAL STABILITY – SL-D001 has superior dimensional stability because linear shrinkage and sinkage are kept to a minimum.
HIGH STRENGTH –SL-D001 patterns will maintain their shape even at elevated ambient temperatures. The patterns will not distort during handling, mounting and shelling.
LOW ASH CONTENT - The ash level is below 0.03% ensuring there is no contamination to the metal.
HIGH PRODUCTION RATE –SL-D001 with good coated performance, no thermal deformation, good fluidity, high surface finish.
GOOD MOLD RELEASE - Mold release is fast and easy.
Application
SL-D001 used in art castings, general cooper alloy castings and coloured glaze.
Technical Specifications
Viscosity at 99 oC IP71 18-25 cps
Penetration at 25oC IP49 5.5-8.5 dmm
Softening Point IP58 62-70.5℃
Drop Melting Point IP 371 65-75℃
Congealing Point IP76 59.5-63℃
Filler Content SPL
Water Content SPL ≤0.18%
Ash Content SPL ≤0.03%
Shrinkage 0.75-0.95%
Form of Supply Pastilles or Slabs
Recommended Parameters
Wax melting temperature 120℃-160℃
Working temperature 80℃-140℃
Features
EXCELLENT DIMENSIONAL STABILITY – SL-D001 has superior dimensional stability because linear shrinkage and sinkage are kept to a minimum.
HIGH STRENGTH –SL-D001 patterns will maintain their shape even at elevated ambient temperatures. The patterns will not distort during handling, mounting and shelling.
LOW ASH CONTENT - The ash level is below 0.03% ensuring there is no contamination to the metal.
HIGH PRODUCTION RATE –SL-D001 with good coated performance, no thermal deformation, good fluidity, high surface finish.
GOOD MOLD RELEASE - Mold release is fast and easy.
Application
SL-D001 used in art castings, general cooper alloy castings and coloured glaze.
Technical Specifications
Viscosity at 99 oC IP71 18-25 cps
Penetration at 25oC IP49 5.5-8.5 dmm
Softening Point IP58 62-70.5℃
Drop Melting Point IP 371 65-75℃
Congealing Point IP76 59.5-63℃
Filler Content SPL
Water Content SPL ≤0.18%
Ash Content SPL ≤0.03%
Shrinkage 0.75-0.95%
Form of Supply Pastilles or Slabs
Recommended Parameters
Wax melting temperature 120℃-160℃
Working temperature 80℃-140℃